03-06-2007 05:35 AM #2
you can save some money by using spi ( southern polyurathane inc.). it's way more user friendly than ppg and a better product in my opinon. i just did a 57 vette using only epoxy , no 2k primer at all. it has been cleared for 90 days and has 0 die back or shrinkage.