Welcome to Club Hot Rod!  The premier site for everything to do with Hot Rod, Customs, Low Riders, Rat Rods, and more. 

  •  » Members from all over the US and the world!
  •  » Help from all over the world for your questions
  •  » Build logs for you and all members
  •  » Blogs
  •  » Image Gallery
  •  » Many thousands of members and hundreds of thousands of posts! 

YES! I want to register an account for free right now!  p.s.: For registered members this ad will NOT show

 

Thread: Lets talk paint product options 32 ford
          
   
   

Results 1 to 15 of 18

Threaded View

  1. #2
    pat mccarthy's Avatar
    pat mccarthy is offline CHR Member/Contributor Visit my Photo Gallery
    Join Date
    Apr 2005
    Location
    bay city
    Posts
    10,546

    i do not care much for dp as a sealer for a show quilty job .fine for production. use many gallons of the stuff . the DBC and the 2002 clear is ok . as for the 2K s primer i used a heavy filler like the k 200 sanded up to 180 wet to 220 grit . last 3 coats then move up to K 36 to finale and colored it if was a poor cover color. wet sand the 36 up to from 320 up to 600 gray back3M wet paper . painted on the 36s no sealer .did many show finishs this way but that been over 10years not sure if ppg still has K36? i move to martin senior primers for a sealer primer .i can go in this in to detail on evey step i have older paint jobs out there that have had very good hold out one is over 20 years old and is a black car . if you want you can PM me and i help much as i can .i had to hang my paint gun up 15 years ago for heath reasons so i not up to speed on some up the new product lines
    Last edited by pat mccarthy; 07-27-2013 at 06:57 PM.
    Irish Diplomacy ..the ability to tell someone to go to Hell ,,So that they will look forward to to the trip

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
Links monetized by VigLink