Here's what I'm using to work the dents out.....the new guy, MP&C, who has the 65 Fairlane build thread suggested using pvc pipe fittings as dollies when working out these dents. They give support around the dented area but don't cause the extra stretching that can occur when hammering on a steel dolly. It's a slow and tedious process but I figure the smoother I can get it the less filler I'll have to use.

IMAG0143_1.jpg

The big shiny area is starting to get pretty flat.
IMAG0144_1.jpg

It actually feels smoother than it looks in this picture. I could probably get away with skim-coating this with filler but I'm gonna try to smooth it out some more first.
IMAG0145_1.jpg