It was a cheapy one. For pulling dents out of 26 gauge tin foil. I bought a pry bar tonight for use on tire repair. It is curved, and rounded on both ends. I heat the crease, and push with the prybar then spray with the water to shrink it. Just have to go slow. Was working on the door last night. I had to take out alot of bondo that was on it to see what it really looked like. I I did the heat and push method, and it seemed to work. There are a few smaller dents that need to be off dollied to flatten it off. In some of it.. The bondo is over 3/4" thick. Right now on the parts I have been working on it is less than 1/16". I still would like to get it better..
A question though.. What do I do for sharp oil canning?? I know of heating a spot in the center of the oil can, and quenching it, but it is like I am chacing the oil can all over the place..