Thread: 41 Willys Gasser project
Threaded View
-
06-13-2013 12:37 PM #11
I'm sorry Steve but I'm receiving flak about discussing your anti roll bar---
But---------you did use a right and a left handed heim joint????????????/
What welding rod do you use to weld stainless to 4130 and do you purge the inside of the tube??????????
I'm assuming that the tube is either .083 at .8129 lbs per feet or .095 at .9182 lbs per ft------------Last edited by jerry clayton; 06-13-2013 at 12:41 PM.





258Likes
LinkBack URL
About LinkBacks
Reply With Quote
This is about the fifth time I’ve tried to reply to this thread. It looks like it’s actually working at the moment.
Where is everybody?