Quote Originally Posted by Bob Parmenter View Post
Never known anyone who successfully double flaired stainless, it's too brittle. Stainless is commonly done single flair with a JIC fitting at 37 degree rather than the 45 degree of the typical mild steel flair. Maybe that's why you had a problem earlier.
You buy the stainless steel tube annealled