Bad looking spots,IE holes in the weld are from bad airflow, or dirt or paint in that spot.

On sheet i just do about a half of an inch at a time, jumping from side to side like torquing down a head. Some guys will have a buddy with them and do a good small bead then follow it up with a hammer and dolly while the bead is still hot.