Thread: Wilwood leaks
          
   
   

Reply To Thread
Results 1 to 15 of 18

Hybrid View

  1. #1
    Dave Severson is offline CHR Member/Contributor Visit my Photo Gallery
    Join Date
    Jul 2003
    Location
    Madison
    Car Year, Make, Model: '67 Ranchero, '57 Chevy, '82 Camaro,
    Posts
    21,160

    Some of the Wilwood pads required a very specific break in procedure, especially the race pads. Even the street ones require a specific number of heat cycles to began to work right.
    Yesterday is history, tomorrow is a mystery, Live for Today!
    Carroll Shelby

    Learning must be difficult for those who already know it all!!!!

  2. #2
    IC2
    IC2 is offline CHR Member Visit my Photo Gallery
    Join Date
    Sep 2007
    Location
    UPSTATE New York
    Posts
    4,336

    This is the process I used, direct from Wilwood:

    "The bedding process is the final "heat cure" for the pads. This final bedding cure differs from an oven heat cure in such that the oven heat cure does not include the pressure, torque, and elevated surface temperatures that are necessary to properly condition the pad for service. As it is with the rotors, new pads must be gradually brought up to temperature and then slowly cooled. If the pads are put into hard service right from the start, damage from fractures or accelerated deterioration due to extreme temperature variations between the surface and the body of the pad can occur. Overall poor performance with the potential for rotor damage are often the results.

    Bedding Steps:

    Once the brake system has been tested and determined safe to operate the vehicle, follow these steps for bedding of all pad materials and rotors.

    1. Begin with a series of 8-10 light stops from approximately 30 MPH down to 15 MPH allowing 20-30 seconds for cooling between each stop.

    2. Progress to series of 8-10 moderate stops from around 45 MPH down to 30 MPH allowing the 20-30 second cool down period between each stop.

    3. Proceed with a series of 8-10 hard stops from 55-65 MPH down to 25 MPH allowing 20-30 seconds of cool down time between each stop.

    4. Drive at a moderate cruising speed, with the least amount of brake contact possible, until most of the heat has dissipated from the brakes. Avoid sitting stopped with the brake pedal depressed to hold the car in place during this time. Park the vehicle and allow the brakes to cool to ambient air temperature."
    Dave W
    I am now gone from this forum for now - finally have pulled the plug

Reply To Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
Links monetized by VigLink