I am going to try some powder coat chrome with a clear powder coat over the chrome layer, it is "suppose" to be 95% as reflective as actual dip. So Im going to try it out before I send off my 6 emblems and drop a quoted 600 bucks. Ill post some before and after pictures, but I was wondering if anyone has tried to fill pot metal pits, and if so what did you use? I was going to try lead but before I did I figured I would ask if anyone has tried this before and make sure it does not booger it up, and if not lead what works the best. I dont have high expectations for the powdercoat to make me happy, but I already have everything so for 28 bucks I figured I would give it the old college try and hope that it suprises me Thanks!