Rule of thumb----use amperage equal to medal thickness--.060=60 amps, .083=83 amps stating point

Purge the bottom side with argon if you can

you didn't say how thick or how long a weld you need to make

I like 1/16 rod and a half second pulse rate for most of the stainless flat or header work I do----